Hydration phase diagram for sodium cobalt oxide Na0.3CoO2*yH2O
| dc.creator | Foo, M. L. | |
| dc.creator | Klimczuk, T. | |
| dc.creator | Cava, R. J. | |
| dc.date | 2004-11-15 | |
| dc.date.accessioned | 2026-07-07T06:24:24Z | |
| dc.date.available | 2026-07-07T06:24:24Z | |
| dc.description | The hydration phase diagram for sodium cobalt oxyhydrate, Na0.3CoO2*yH2O (y=0, 0.6, 1.3), was determined as a function of relative humidity at 298K. It is found that greater than 75% relative humidity is needed for complete hydration of anhydrous Na0.3CoO2 to the superconducting phase Na0.3CoO2*1.3H2O. Dehydration studies show that a minimum of 43% relative humidity is needed to maintain the stability of the fully hydrated superconducting phase. The intermediate hydrate, Na0.3CoO2*0.6H2O, is stable between 10% and 50% relative humidity on hydration, and 35% to 0% relative humidity on dehydration. | |
| dc.description | submitted to Mat. Res. Bull., 4 pages, 4 figures | |
| dc.identifier | https://arxiv.org/abs/cond-mat/0411387 | |
| dc.identifier | http://arxiv.org/abs/cond-mat/0411387 | |
| dc.identifier | Material Research Bulletin vol. 40/4 (2005), p. 665-670 | |
| dc.identifier.uri | http://salesiana.dossiersoluciones.com/handle/123456789/96528 | |
| dc.subject | Superconductivity | |
| dc.title | Hydration phase diagram for sodium cobalt oxide Na0.3CoO2*yH2O | |
| dc.type | text |