Supercooling and the Metal-Insulator Phase Transition of NdNiO$_{3}$

dc.creatorKumar, Devendra
dc.creatorRajeev, K. P.
dc.creatorAlonso, J. A.
dc.creatorMartinez-Lope, M. J.
dc.date2007-12-24
dc.date2008-01-10
dc.date.accessioned2026-07-07T08:53:25Z
dc.date.available2026-07-07T08:53:25Z
dc.descriptionWe report the temperature and time dependence of electrical resistivity on high temperature, high oxygen pressure prepared polycrystalline samples of NdNiO_3. NdNiO_3 is metallic above 195 K and below that temperature it undergoes a transition to an insulating state. We find that on cooling NdNiO_3 below 195 K it goes into a state which is not in thermodynamic equilibrium and slowly relaxes over several hours. As we cool it further and go below about 110 K it goes into a stable insulating state. On heating the system from the insulating state towards 200 K we find that it remains stable and insulating and undergoes a rather sharp insulator to metal transition in the temperature range 185 K to 195 K. We try to make sense of these and a few other interesting observations on the basis of our current understanding of first order phase transitions, supercooling, and metal-insulator transitions.
dc.description8 pages, 6 figures
dc.identifierhttps://arxiv.org/abs/0712.3990
dc.identifierhttp://arxiv.org/abs/0712.3990
dc.identifier.urihttp://salesiana.dossiersoluciones.com/handle/123456789/145618
dc.subjectOther Condensed Matter
dc.titleSupercooling and the Metal-Insulator Phase Transition of NdNiO$_{3}$
dc.typetext

Files

Collections