Beta-NMR of Isolated Lithium in Nearly Ferromagnetic Palladium
| dc.creator | Parolin, T. J. | |
| dc.creator | Salman, Z. | |
| dc.creator | Chakhalian, J. | |
| dc.creator | Song, Q. | |
| dc.creator | Chow, K. H. | |
| dc.creator | Hossain, M. D. | |
| dc.creator | Keeler, T. A. | |
| dc.creator | Kiefl, R. F. | |
| dc.creator | Kreitzman, S. R. | |
| dc.creator | Levy, C. D. P. | |
| dc.creator | Miller, R. I. | |
| dc.creator | Morris, G. D. | |
| dc.creator | Pearson, M. R. | |
| dc.creator | Saadaoui, H. | |
| dc.creator | Wang, D. | |
| dc.creator | MacFarlane, W. A. | |
| dc.date | 2007-01-17 | |
| dc.date.accessioned | 2026-07-07T07:43:11Z | |
| dc.date.available | 2026-07-07T07:43:11Z | |
| dc.description | The temperature dependence of the frequency shift and spin-lattice relaxation rate of isolated, nonmagnetic Li-8 impurities implanted in a nearly ferromagnetic host (Pd) are measured by means of beta-detected nuclear magnetic resonance (b-NMR). The shift is negative, very large and increases monotonically with decreasing T in proportion to the bulk susceptibility of Pd for T > T*~ 100 K. Below T*, an additional shift occurs which we attribute to the response of Pd to the defect. The relaxation rate is much slower than expected for the large shift and is linear with T below T*, showing no sign of additional relaxation mechanisms associated with the defect. | |
| dc.description | 4 pages, 3 figures | |
| dc.identifier | https://arxiv.org/abs/cond-mat/0701394 | |
| dc.identifier | http://arxiv.org/abs/cond-mat/0701394 | |
| dc.identifier | Phys. Rev. Lett. 98, 047601 (2007) | |
| dc.identifier | doi:10.1103/PhysRevLett.98.047601 | |
| dc.identifier.uri | http://salesiana.dossiersoluciones.com/handle/123456789/122726 | |
| dc.subject | Materials Science | |
| dc.title | Beta-NMR of Isolated Lithium in Nearly Ferromagnetic Palladium | |
| dc.type | text |