dc.descriptionThermopower measurements have been carried out on the Ni substituted samples of Na0.75CoO2 in the temperature range 4.2K to 300K. The room temperature TEP increases by 20microV/K even with 1% Ni substitution and systematically increases with increasing Ni content upto 5%. The increase in TEP is accompanied by a decrease in rho, thus increasing the ratio of S^(2)/rho on Ni substitution. At low T, the TEP shows an anomaly in the substituted samples, showing a peak at T ~ 20K.
dc.descriptionTo appear in Sol. St. Phys.India Vol 50 (2005)
dc.identifierhttps://arxiv.org/abs/cond-mat/0510342
dc.identifierhttp://arxiv.org/abs/cond-mat/0510342
dc.identifier.urihttp://salesiana.dossiersoluciones.com/handle/123456789/102752
dc.subjectStrongly Correlated Electrons
dc.subjectMaterials Science
dc.titleEnhanced thermopower upon Ni substitution in Na0.75CoO2
dc.typetext

Files

Collections