Formation of ferromagnetic bulk amorphous Fe40Ni40P14B6 alloys
| dc.creator | Li, Qiang | |
| dc.date | 2006-11-27 | |
| dc.date.accessioned | 2026-07-07T07:31:29Z | |
| dc.date.available | 2026-07-07T07:31:29Z | |
| dc.description | Ferromagnetic bulk amorphous Fe40Ni40P14B6 alloy rods with a diameter of 1.2 mm can be prepared by means of a rapid quenching technique. If a fluxing technique is also used, amorphous rods with a diameter as large as 2.5 mm can be synthesized. The critical cooling rate Rc for the glass formation Fe40Ni40P14B6 is estimated to be on the order of 100 K.s-1 | |
| dc.description | 20 pages, 5 figures, 1 table | |
| dc.identifier | https://arxiv.org/abs/cond-mat/0611661 | |
| dc.identifier | http://arxiv.org/abs/cond-mat/0611661 | |
| dc.identifier | Materials Letters, 2006, 60(25-26): 3113-3117 | |
| dc.identifier | doi:10.1016/j.matlet.2006.02.054 | |
| dc.identifier.uri | http://salesiana.dossiersoluciones.com/handle/123456789/118770 | |
| dc.subject | Materials Science | |
| dc.title | Formation of ferromagnetic bulk amorphous Fe40Ni40P14B6 alloys | |
| dc.type | text |